Rapid Sintering 3D Ultra Multilayer Dental Zirconia Block– 20 Minutes Fast Sintering

High-quality multilayer zirconia block with rapid sintering in 20 minutes.

Perfect for dental labs seeking strength, translucency, and natural aesthetics.

Contact us for wholesale prices.

Deal of the Day

Description

Rapid Sintering Zirconia Block Multilayers

Rapid sintering zirconia blocks are advanced multilayer dental materials designed for both speed and performance. With ultra-fast sintering cycles as short as 20 minutes, they significantly improve efficiency in dental laboratories. The multilayer gradation structure provides natural translucency, strength, and color transition for lifelike restorations.

Manufactured with premium zirconia powder(Tosoh), these blocks deliver accuracy, durability, and esthetic satisfaction for crowns, bridges, and full-arch cases.

Features

  • Ultra-Fast Sintering: Complete sintering in as little as 20 minutes, boosting lab productivity.

  • High Flexural Strength:

    • Enamel Layer: ~800 ±100 MPa

    • Transition Layer: ~950 ±100 MPa

    • Cervical Layer: ~1100 ±100 MPa

  • Excellent Translucency: 44–51% light transmission, delivering lifelike esthetics.

  • Multilayer Gradation: Smooth transition from cervical to incisal for natural appearance.

  • Premium Zirconia Powder: Sourced from Japan, ensuring stability and high quality.

  • Low Shrinkage Rate: Precise fit and increased crown milling capacity

Sintering Programming Setting

Phase Target Temperature (°C) Heating/Cooling Rate (°C/min) Hold Time (minutes) Purpose
Start Temperature 25 0 Ambient starting point (room temperature)
Set Temp 1 (T1) 1000 250 0 Rapid preheat to remove binders/solvents
Set Temp 2 (T2) 1300 80 0 Intermediate temperature for densification
Set Temp 3 (T3) 1440 40 5 Peak sintering temperature (full densification & crystallization)
Set Cool 1 (C1) 700 100 5 Controlled cooling to avoid thermal shock

Key Notes for Technicians:

✅ Total Cycle Time: ~20 minutes (per manufacturer’s “super fast” claim).
⚠️ Critical Phases:

  • T3 (1440°C): Must hold for 5 minutes to ensure complete sintering and optimal mechanical properties.
  • Cooling (C1): Slow, controlled cooling (100°C/min) with a 5-minute hold at 700°C minimizes internal stresses and prevents cracking.
    📏 Accuracy: Follow rates and temperatures precisely—deviations may compromise strength or fit.